MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ravago Manufacturing Americas Aquatuf® HMP-335 (Roto) HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HMP-335 is a high-density polyethylene compound designed for applications like kayaks or boats that require a balance high stiffness and extreme toughness.

Key Features: 35-mesh powder; Good moldability; Excellent long term outdoor weatherability (UV15); Superior balance of toughness and rigidity; High stiffness; Excellent low temperature impact; Compounded for uniform additive dispersion; Natural as well as standard, custom or special effect colors available; Stock colors may be available. See Stock color bulletin; Also available in pellet form as HM-335

Availability: North America

Features: Good Moldability; Good Weather Resistance; High Stiffness; Low Temperature Impact Resistance; Ultra High Toughness

Appearance: Colors Available; Natural Color

Form: Powder

Processing Method: Rotational Molding

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.380 g/cc0.0137 lb/in³35-mesh powder; ASTM D1895
Density 0.946 g/cc0.0342 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.4 MPa3100 psiRotational Molded; ASTM D638
Elongation at Break >= 400 %>= 400 %Rotational Molded; ASTM D638
Flexural Modulus 0.896 GPa130 ksiTangent, Rotational Molded; ASTM D790
Impact Test 92.2 J
@Temperature -40.0 °C
68.0 ft-lb
@Temperature -40.0 °F
Rotational Molded, F50
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO4850 / 311543

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.