MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Estane® 3D TPU F95A-030 BR ECO PL TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Product Description: Type: Polyether Thermoplastic Polyurethane (TPU); Features: Properties similar to standard TPU of same hardness, sustainable solution with broad printing window, over 30% bio-based content; Uses: 3D Printing using Fused Filament Fabrication (FFF) technology

Availability: Asia Pacific; Latin America; North America

Features: Renewable Resource Content

Uses: Additive Manufacturing (3D printing)

Form: Pellets

Processing Method: 3D Printing, Fused Filament Fabrication (FFF)

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95
@Time 5.00 sec
ISO 868
Tensile Stress 2760 psiZY Orientation; ISO 527-2
 5800 psiXZ Orientation; ISO 527-2
 1310 psi
@Strain 50 %
XZ Orientation; ISO 527-2
 1600 psi
@Strain 100 %
XZ Orientation; ISO 527-2
 4350 psi
@Strain 300 %
XZ Orientation; ISO 527-2
Elongation at Break 240 %ZY Orientation; ISO 527-2
 390 %XZ Orientation; ISO 527-2
 
Processing PropertiesOriginal ValueComments
Zone 1 392 °F
Zone 2 401 °F
Zone 3 410 °F
Zone 4 410 °F
Die Temperature 401 °F
Drying Temperature 212 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBRZ782 / 311475

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.