Features: • Soluble green light-emitting spiro-copolymer. • High efficiency. • Long lifetime, with further potential to improve. • Saturated green color coordinates, with low operation voltage.
Typical performance measured in standard device stack (ITO/PEDOT:PSS 20 nm/SPG-01T 80 nm/Ba 6 nm/Ag 150 nm): • Max. efficiency: 11 Cd/A. • V_on: 2.5 V. • V at 100 cd/m2: 3.6 V. • V at 1000 cd/m2: 6.0 V. • Max. power eff.: 12 lm/W. • External quantum eff.: 4.1%. • CIE1931 at 100 cd/m2: (0.33, 0.59). • DC lifetime at 100 cd/m2 at RT: >10k hrs. • AC lifetime at 200 cd/m2 at RT: >5000 hrs.Synonyms: Livilux™ SPG-01T Alfa Chemistry Materials product group: Organic Light-Emitting Diode (OLED) Materials Manufacturer data sheet |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |