Product Description: 50% Glass Fiber, Heat Stabilized, Bio-based polyamide 5.6 Resin ID (ISO 1043): PAGF50 Filler / Reinforcement: Glass Fiber, 50% Filler by Weight Additive: Heat Stabilized Processing: Injection Molding Color: Grey Information provided by Petropol |