Compound 9646 is a 60 durometer black colored Fluorinated Hydrocarbon elastomer. It exhibits excellent resistance to heat, compression set, petroleum based oils, aliphatic and aromatic fuels. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 615 A1-10 B37 B38 EF31 EO78 F15; 4 HK 615 A1-11 B38 EF31 EO78; 6 HK 615 A1-10 A1-11 B31 B38 EF31 EO88 F15 This Compound is RoHS Compliant Information provided by Pressure Seals Inc. |