MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi TPU98A 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: TPU98A is a specifically formulated flexible filament for easy & high-speed printing on both direct and Bowden style 3D printers. TPU98A does not require the use of a heated bed and can even be printed straight onto (clean) glass.TPU98A is the flexible filament for (semi) professional users who do not want to compromise and require a high mechanical flexible filament that prints easily. TPU98A is an extremely usable flex-filament with a wide variety of different applications such as Orthopedic insoles, Prosthetics, Vibration dampers and much more.

Features:

  • Strong & flexible
  • Works on direct & Bowden style 3D printers
  • Printable at speeds of >75mm/s
  • Exceptionally high softening point of 138°C
  • 450% elongation at break
  • Resistance to oils, greases & microorganisms
  • Easily print watertight objects
Colors: TPU98A is available from stock in 6 colors.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccISO 1183
Filament Diameter 1750 µmTolerance: 50 µm, =95% Roundness
 2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 57 g/10 min
@Load 10.0 kg,
Temperature 210 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ISO 7619-1
Tensile Strength, Yield 50.0 MPaISO 527
Elongation at Break 450 %ISO 527
Tensile Modulus 150 MPa(E); ISO 527
Charpy Impact, Notched NBISO 179 1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CISO 294
Vicat Softening Point 138 °CISO 306
Glass Transition Temp, Tg -16.0 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 240 °CPrinting Temperature
 
Descriptive Properties
Bed Temp=60°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9851 / 301076

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.