MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Signlok 406 Adhesive System
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD® 406 acrylic adhesive in combination with LORD Accelerator 19 or 19GB can be used to replace welding, brazing, riveting and other mechanical fastening methods. This adhesive system performs particularly well in low-temperature environments and applications that are subject to high impact or high peel loads. LORD 406 acrylic adhesive, when mixed with LORD Accelerator 19 or 19GB, creates an adhesive system that bonds a wide variety of prepared or unprepared metals and engineered plastics. The adhesive system is specifically formulated to provide the highest impact and peel strengths available in a room temperature curing adhesive. LORD 406 acrylic adhesive can be mixed with either LORD Accelerator 19 or LORD Accelerator 19GB. LORD Accelerator 19 improves the high temperature resistance of LORD 406 acrylic adhesive, and is available in off-white or black. LORD Accelerator 19GB allows precise control of the adhesive bondline thickness due to its content of glass beads. LORD Accelerator 19GB is available in off-white, red or grey. LORD 406 acrylic adhesive is flammable. Do not store or use near heat, sparks or open flame.

Features: bonds a wide range of unprepared metals with minimal substrate preparation, as well as engineered thermoplastics including XENOY®, polycarbonate, ABS and acrylics. performs at temperatures from -40°F to +300°F (-40°C to +149°C). resists dilute acids, alkalis, solvents, greases, oils, moisture, salt spray and weathering; provides excellent resistance to indirect UV exposure. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility. when mixed with LORD Accelerator 19, adhesive system is UL 746C certified.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.25 - 9.55 lb/galAdhesive
 12.15 - 13.2 lb/galAccelerator
Solids Content 100 %mixed
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2000 psiCured, Lap, Aluminum
 2300 psiCured, Lap, Steel
Peel Strength 20.0 - 23.0 pliversus aluminum
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 15.0 °CAdhesive
 >= 93.0 °CAccelerator
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 24.0 °C
Pot Life 12.0 - 17.0 min
@Temperature 24.0 °C
time to handling strength, mixed with 406 Accelerator, 50 psi Shear
Working Life 6.00 - 10.0 min
@Temperature 24.0 °C
Mixed with 406 Accelerator
Shelf Life 18.0 Month
@Temperature 4.00 - 10.0 °C
in original, unopened container
 
Descriptive Properties
AppearanceOff-White Paste
 Tan Paste
Cured AppearanceTan to GreenMixed with 406 Accelerator
Mix Ratio2 to 1by volume, Adhesive to Accelerator
Mixed AppearanceTan PasteMixed with 406 Accelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9148 / 232536

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.