This is a general purpose elastamax based on SEBS technology. It exhibits low gloss, low density and a tacky surface. Physical Form: Pellet. Standard Color: Black. Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |