MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC Valox® 420M PBT (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.

This data was supplied by SABIC-IP for the Asia Pacific region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D 792
Water Absorption 0.060 %
@Time 86400 sec
ASTM D 570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC Method
 0.0050 - 0.0080 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC Method
 0.0060 - 0.0080 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D 785
Tensile Strength at Break 119 MPaType I, 5 mm/min; ASTM D 638
Flexural Strength 189 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 7580 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 85.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 8.01 J/cm
@Temperature 23.0 °C
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 3.20e+16 ohm-cmASTM D 257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D 150
 3.8
@Frequency 100 Hz
ASTM D 150
Dielectric Strength 18.7 kV/mm
@Thickness 3.20 mm
in air; ASTM D 149
 24.8 kV/mm
@Thickness 1.60 mm
in oil; ASTM D 149
Dissipation Factor 0.0020
@Frequency 100 Hz
ASTM D 150
 0.020
@Frequency 1e+6 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 25.2 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 6.40 mm
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silberline Silvet® 420-20-P
Overview of materials for Polyetheretherketone, Unreinforced
Dow DMDA-8007 NT 7 High Density Polyethylene Resin

PSABIC4673 / 118561

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.