MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ASI® MP 55320 Methacrylate adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: MP55320 is a high performance two part methacrylate adhesive engineered to bond a wide range of plastics, metals, and composite assemblies. It offers outstanding bond strength, is extremely durable, with excellent impact and weathering properties. MP55320 greatly increases the reliability of finished assemblies with exceptional flexibility, its ability to with stand extreme temperature fluctuation and thermal cycling, and resistance to a wide range of chemicals and environmental conditions.

Substrates bonded include ABS, Acrylic, Aluminum, Nylon, Phenolic, Polycarbonate, Polystyrene, PVC, Steel, Stainless metals, coated metals, fiberglass, phenolics, gel coats, epoxy, rim urethane, polyurethane, liquid molding resins, PPO's, Vinyl, PEEK, PBT Blends, and PET Blends.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/galuncured, mixed
Viscosity 50000 cP
@Temperature 25.0 °C
activator, uncured
 130000 cP
@Temperature 25.0 °C
resin, uncured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 2500 psicured
Shear Strength 2500 - 2800 psicured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -67.0 °F
Flash Point 51.0 °Funcured
 
Processing PropertiesOriginal ValueComments
Working Life 12.0 min
 
Descriptive Properties
Color / appearanceoff white, amber shell. Uncured.
Gap Fillup to 0.25 inches. Cured
Handling Strength25 minutes, cured
Mix Ratio10 to 1. (Vol or wt). Uncured
Thix Index5. Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9020 / 233387

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.