MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber HN 36 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: HN-36 is a halogen–free, medium-coarse particle size ATH product that provides low cost flame retardant and smoke suppression in a variety of applications. The particle size distribution is specifically designed for low viscosity, high filler loading levels, and excellent processing characteristics, up to 200°C.

Applications: HN-36 is recommended for rubber goods, compression molded thermosets, coatings, adhesives, latex, vinyl and urethane compounds and carpet backings.

Physical Form: White powder

Morphology: Hexagonal Platelets

Generic Type: Aluminum Hydroxide

CAS No.: 21645-51-2

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 1.20 g/ccpacked
Brightness 93 %
Oil Absorption >= 21 %21 ml/100gm
Particle Size <= 10 µmScreen Analysis: 36.2 percent
 19 µmMedian Particle Diameter
 <= 45 µmScreen Analysis: 77.1 percent
 <= 150 µmScreen Analysis: 100 percent
Specific Surface Area 140 m²/gBET
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 3.0
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 7700 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 <= 0.020 %
Free Water 0.14 %
@Temperature 105 °C
TGA
Loss on Ignition(%) 34.5 %
@Temperature 550 °C
Na2O 0.020 %soluble
 0.20 %total
SiO2 <= 0.040 %
 
Descriptive Properties
Al(OH)3 (%)99.6
CIELAB, L*97
ColorWhite powder
FunctionalityFunctionality
 Functionality
 Functionality: Thermal properties
 Smoke Suppression
Functionality: Adsorption & FiltrationFunctionality: Adsorption & Filtration
Functionality: Electrical PropertiesFunctionality: Electrical Properties
Functionality: Mechanical hardnessFunctionality: Mechanical hardness
Functionality: Optical effectsFunctionality: Optical effects
Functionality: Thermal resistanceFunctionality: Thermal resistance
Market/Application: Building & ConstructionAdhesives, Caulks & Sealants
 Market/Application: Building & Construction
Market/Application: E & E, InfrastructureMarket/Application: E & E, Infrastructure
Market/Application: IndustrialMarket/Application: Industrial
Market/Application: ThermoplasticsMarket/Application: Thermoplastics
Market/Application: ThermosetsMarket/Application: Thermosets
Market/Application: TransportationMarket/Application: Transportation
Market/Application: Wire and CableMarket/Application: Wire and Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER700 / 300806

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.