System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Wefapress Cera Flex PE-UHMW
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
UHMW PE (Ultra High Molecular Weight PE)
Material Notes:
Properties: High wear resistance, Flexible over a wide angle range.
Applications: Lining material. Industries: Bulk industry.
Information provided by Wefapress.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.950
g/cc
DIN ISO 1183
Moisture Absorption
<= 0.0100 %
Molecular Weight
<=
4.00e+6
g/mol
Mechanical Properties
Original Value
Comments
Hardness, Shore D
64
@Time 15.0 sec
DIN 53505
Ball Indentation Hardness
38.0
MPa
@Time 30.0 sec
DIN ISO 2039 Teil 1
Tensile Strength
>=
16.0
MPa
DIN 53455
Tensile Strength, Ultimate
110
MPa
DIN ISO 178
Elongation at Break
>= 25 %
DIN ISO / R 527
Modulus of Elasticity
0.750
GPa
DIN 53457
Charpy Impact, Notched
>=
100
kJ/m²
DIN ISO 179
Coefficient of Friction
0.20
Sand Slurry
105
% Abrasion
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+13
ohm
IEC 60093
Dielectric Strength
45.0
kV/mm
IEC 60243
Thermal Properties
Original Value
Comments
CTE, linear
200
µm/m-°C
Specific Heat Capacity
1.70
J/g-°C
Thermal Conductivity
0.350
W/m-K
DIN 52612
Melting Point
135
°C
DIN ISO 3146
Maximum Service Temperature, Air
47.0
°C
Dimensional Stability; DIN 53461
80.0
°C
Continuous Application Temp.
Vicat Softening Point
81.0
°C
DIN 53460
Minimum Service Temperature, Air
-200
°C
Flammability, UL94
HB
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PWEFA929 / 243134
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.