MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ITW Chockfast® Red SG Epoxy Grouting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: 100% solids epoxy grouting compound which is used to grout large machinery and to support soleplates in all types of foundation designs with clearances as little as 1” (25mm). CHOCKFAST RED SG has extremely high physical properties and negligible shrinkage, making it ideal for final positioning of critically aligned equipment within close tolerances. Skid mounted compressors, extruders, turbines, pumps, motors and crane rails are just a few types of equipment supported on CHOCKFAST RED SG. When using CHOCKFAST RED SG for crane rail applications expansion joints may be placed every 10’ (3m).

USE & BENEFITS CHOCKFAST RED SG has the following advantages when compared to conventional cementitious grouts: • Impervious to oil and chemical attack • Cures at least three times as quickly • Pre-packaged unit • Grout machinery in final aligned position• Higher physical strengths • Strong bond to metal and concrete • Unaffected by weathering and freeze/thaw cycling • Superior resistance to fatigue CHOCKFAST RED SG contains no non-reactive diluents which could interfere with the curing mechanism or which could cause material loss during or after cure. Machinery may be positioned at its final elevation before pouring because the shrinkage is negligible. Critical alignments are maintained during machinery operation due to CHOCKFAST RED SG’s high dimensional stability and resistance to creep and vibration.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.24 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2130 psiASTM D638
Flexural Strength 4800 psiASTM C580
Flexural Modulus 2.62e+6 psiASTM C580
Compressive Strength 18120 psiASTM C579 MOD
Compressive Modulus 1.97e+6 psiASTM C579 MOD
Izod Impact, Notched 0.600 ft-lb/inASTM D258
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.8 µin/in-°F
@Temperature 0.000 - 60.0 °C
ASTM D696
Maximum Service Temperature, Air 140 °F
Shrinkage 0.00 %Not measurable; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 48.0 hour
@Temperature 21.0 °C
approximate
Pot Life 60.0 min
@Temperature 21.1 °C
Shelf Life 24.0 MonthIn dry storage
 
Descriptive Properties
Fire Resistanceself extinguishingASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9023 / 239533

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.