System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical LUMIPLAS LD8550I Light diffusion ABS, Injection grade
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Extruded
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Light diffusion, Weatherability
Application: (LED) Lamp cover, Signboard, Lighting decoration of electronic device
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.20
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.0050
-
0.0080
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
33
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
630
kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break
>= 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Strength
93.2
MPa
@Thickness 6.40 mm
15mm/min; ASTM D790
Flexural Modulus
23000
kg(f)/cm²
@Thickness 6.40 mm
15mm/min; ASTM D790
Izod Impact, Notched
15.0
kg-cm/cm
@Thickness 3.20 mm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
126
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical
120
°C
UL 746B
UL RTI, Mechanical with Impact
105
°C
UL 746B
UL RTI, Mechanical without Impact
120
°C
UL 746B
Flammability, UL94
V-2
@Thickness 0.500 mm
V-2
@Thickness 1.60 mm
V-2
@Thickness 2.50 mm
V-2
@Thickness 3.00 mm
Optical Properties
Original Value
Comments
Transmission, Visible
57 %
@Thickness 1.00 mm
JIS K7361
Processing Properties
Original Value
Comments
Rear Barrel Temperature
250
-
270
°C
Middle Barrel Temperature
260
-
280
°C
Front Barrel Temperature
270
-
290
°C
Nozzle Temperature
270
-
290
°C
Melt Temperature
280
-
300
°C
Mold Temperature
60.0
-
100
°C
Drying Temperature
100
-
120
°C
@Time 10800 - 18000 sec
Moisture Content
<= 0.020 %
Back Pressure
0.981
-
3.92
MPa
Screw Speed
40
-
70
rpm
Descriptive Properties
Outdoor Suitability
f1
UL746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLHCHEM9801 / 239317
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.