MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vinnolit® S 100 Suspension PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: High K-value suspension PVC for thermoplastic processing of PVC. Vinnolit® S 100 is a specialty product for the production of flexible PVC-articles with improved plasticizer acceptance and excellent mechanical performance, particularly for rubberlike gaskets with matte surface. Vinnolit® S 100 is a free-flowing powder with very high porous particles. It may be processed with all standard additives such as plasticizers, stabilizers, lubricants, fillers and pigments similarly to an S-PVC with a lower K-value. Vinnolit® S 100 is mixed by the standard hot or cold mixing methods. Recommended temperatures are 120 °C in the heating mixer and 40 °C in the cooling mixer. Due to the very high porosity even plasticizers with longer side chains can be accepted by the particles easily which leads to significantly improved mixing cycles. Vinnolit® S 100 may be processed in the form of a blend or granules on all standard equipment, such as extruders, injection molding machines and calenders. Small amounts of Vinnolit® VK 710 may be added to the blend to facilitate fusion.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.30 %ISO 1269
Apparent Bulk Density 0.440 g/ccISO 60
Particle Size >= 63 µm>=85% Retained on 0.063 mm Sieve; ISO 4610
 <= 250 µm<= 2% Retained on 0.25 mm Sieve; ISO 4610
Viscosity Test 2.93 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
K-Value99ISO 1628-2
Plasticizer Absorption (%)45ISO 4608. At room temperature.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO908 / 291105

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.