MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Alfa Chemistry Materials Vinyl Chloride
Material Notes: Solubility: Slightly soluble; In water, 8.8X10+3 mg/L at 25 ?; In water, 2700 mg/L; Soluble in ethanol; very soluble in ethyl ether; Soluble in carbon tetrachloride and benzene; Soluble in hydrocarbons, oil, chlorinated solvents, and most common organic solvents.; HIGH MOL WT UNMODIFIED PVC SOL IN: CYCLOHEXANONE; METHYL CYCLOHEXANONE; DIMETHYL FORMAMIDE; NITROBENZENE; TETRAHYDROFURAN; ISOPHORONE; MESITYL OXIDE; LOW MOL WT PVC POLYMERS SOL IN: DIPROPYL KETONE; METHYL AMYL KETONE; METHYL ISOBUTYL KETONE; ACETONYLACETONE; METHYL ETHYL KETONE; DIOXANE; METHYLENE CHLORIDE; Solubility in water, g/l at 25 ?: 1.1 (poor); Solubility in water: very poor; (77°F): 0.1%

Stability: An unstable polyperoxide is apparently formed in vinyl chloride through oxidation by atmospheric oxygen in the presence of any of a variety of contaminants. Storage under these conditions for a long period increases the concentration of unstable polyperoxide to hazardous levels.; Long-term exposure to air may result in formation of peroxides that can initiate explosive polymerization of the chloride.; STABILIZERS ARE NECESSARY TO PREVENT DISCOLORATION FROM EXPOSURE TO LIGHT OR HEAT;AT ORDINARY TEMPERATURES IT MAY UNDERGO SLOW DEHALOGENATION WITH EVOLUTION OF HYDROGEN CHLORIDE

Alfa Chemistry Materials product group: Polymer Science

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 0.01072 cP
@Temperature 20.0 °C
Gas
 0.28 cP
@Temperature -20.0 °C
Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZZALFA67538 / 305185

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.