MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-9062 Fluoroelastomer Terpolymer, 71% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-9062 is a low viscosity, peroxide curable terpolymer designed for injection molding. It provides excellent mold flow and easy removal of molded parts. Properly compounded and cured, DAI-EL® G-9062 has excellent compression set, chemical and steam resistance.

Typical Applications: O-Rings and seals

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/cc
Mooney Viscosity 23
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
Tensile Strength at Break 20.6 MPa
Elongation at Break 220 %
100% Modulus 4.60 MPa
@Strain 100 %
Compression Set 12 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -8.00 °CLow Temperature Retraction, TR10
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 180 °C
Post cure
 10.0 min
@Temperature 160 °C
Press Cure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 71 %
 
Descriptive Properties
ColorWhite to light pink
Test Formula1.5 phrPeroxide
 100 phrDAI-EL® G-9062
 20 phrMT Carbon Black (N-990)
 4 phrTAIC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIJ9861 / 209932

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.