MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dow™ DFDA-7059 NT7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: Dow DFDA-7059 NT7 linear low density polyethylene is an ethylene-butene copolymer which is supplied in pellet form. It is generally recommended for slot cast thin film applications requiring both clarity and toughness. It is excellent in coextruded, slot cast stretch wrap. This resin is also suitable for use in hose and tube applications.
Main Characteristics:
  • High clarity
  • High tensile strength
  • High elongation
  • Good puncture resistance
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU No 10/2011. Consult the regulations for complete details.

Availability: Europe; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU No 10/2011

Form: Pellets

Processing Method: Blown Film; Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1490 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 1380 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Film Elongation at Break, MD 450 %
@Thickness 0.0254 mm
Cast Film; ASTM D882
Film Elongation at Break, TD 850 %
@Thickness 0.0254 mm
Cast Film; ASTM D882
Elongation at Break 570 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 11 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 32000 psi2% Secant, Plaque molded and tested in accordance with ASTM D4976; ASTM D790B
Elmendorf Tear Strength MD 50 g
@Thickness 0.0254 mm
Cast Film; ASTM D1922
Elmendorf Tear Strength TD 400 g
@Thickness 0.0254 mm
Cast Film; ASTM D1922
Dart Drop Test 70.0 g
@Thickness 0.0254 mm
Cast Film; ASTM D1709A
Film Tensile Strength at Break, MD 5000 psi
@Thickness 0.0254 mm
Cast Film; ASTM D882
Film Tensile Strength at Break, TD 3600 psi
@Thickness 0.0254 mm
Cast Film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °F
 
Optical PropertiesOriginal ValueComments
Haze 2.5 %
@Thickness 0.0254 mm
Cast Film; ASTM D1003
Gloss 92 %
@Thickness 0.0254 mm
45°, Cast Film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 520 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF478 / 311171

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.