PA66 reinforced with 15% glass fiber, suitable for moldings used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electro tools, electromotor, cooling screws of blowers, gear wheels, carrying parts in the automotive industry like e.g.. brake cables. Delivered in black color. Information Provided by Plastcom spol. s r.o. |