MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Less Common Metals Tb-Fe-Co Cast Magneto-Optic Alloy
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: Magneto-Optic terbium-iron-cobalt based alloys. Produced to a high degree of compositional control and with very low levels of critical impurities such as oxygen.

Alloying Additions: Gadolinium may be used as a substitute for terbium; tantalum and/or chromium are common additions to Tb-Fe-Co systems.

Form: Routinely supplied in the form of powder, milled to a specific size requirement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.020 %
Calcium, Ca <= 0.010 %
Carbon, C <= 0.0050 %
Cobalt, Co 3.0 - 8.0 %
Iron, Fe 21.875 - 57 %
Other, each <= 0.020 %
Oxygen, O <= 0.050 %
Silicon, Si <= 0.020 %
Terbium, Tb 40 - 70 %Gadolinium may be substituted

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Less Common Metals Tb-Fe-Co Cast Magnetostrictive Alloy
Carpenter Thermo-SpanĀ® Fe-Co-Ni Superalloy
304 Stainless Steel

NLCM06 / 17975

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.