MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® HTplus M1035 P1 black Polyphthalamide (PPA), 50% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Glass fiber-reinforced polyphthalamide compound for injection molding. VESTAMID® HTplus M1035 P1 black is a glass fiber-reinforced (50%), heat-stabilized polyphthalamide compound (PPA) with high flow ability for injection molding. This compound is especially suitable for manufacturing parts subjected to high mechanical performance at high temperature, especially burst pressure applications. VESTAMID® HTplus M1035 P1 black is supplied as cylindrical pellets in polyethylene packaging. Drying at 120°C for at least 4 hours before processing is recommended.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccISO 1183
Water Absorption 4.0 %Sim. to ISO 62
Moisture Absorption 0.200 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 240 MPaISO 527
Elongation at Break 1.6 %ISO 527
Tensile Modulus 17800 MPaISO 527
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -40.0 °C
Complete Break; ISO 179/1eU
 61.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Dielectric Strength 29.0 kV/mmSim. to IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2.
Melting Point 310 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 305 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 293 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 230 °CLoad C; ISO 75-1/-2
Vicat Softening Point 288 °CMethod B: 10 N, 50 K/h; ISO 306
 308 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 120 °CISO 11357-1/-2
Flammability Test 1.0
@Thickness 1.60 mm
IEC 60695-11-10
 1.0
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 340 °CTest condition for mold shrinkage

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450GL30 Blk Polyetheretherketone, 30% Glass Fiber, Black
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30% Glass Fiber Reinforced Molding Grade
DuPont Mobility and Materials Vespel® CP-0648 Polyimide
DuPont Mobility and Materials Vespel® CP-0301 Fiber Compound
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35

PEVONIK836 / 243045

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.