Description: Apcoflex® N285 is a cold polymerized co-polymer of acrylonitrile and butadiene. It contains non-staining antioxidant. Applications: Apcoflex® N285 is an medium viscosity grade and is intended to be used in applications where the requirement for flexibility at sub-freezing temperatures is greater than that can be achieved with medium ACN grades such as N745.. It finds extensive applications in Hoses, Profiles, moulded Rubber goods for automotive and industrial applications. CAS No,: 9003-18-3 Information provided by Apcotex Industries Limited |