MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer FL2000 PC (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24" (6.0mm) wall. This product offers low temperature impact strength and high heat resistance in combination with LEXAN FL2000 resin is available in opaque colors only.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccfoam molded; ASTM D792
 1.21 g/ccASTM D792
Water Absorption 0.13 %
@Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 0.34 %ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 6.40 mm
SABIC method
Melt Flow 10.3 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Chemical PropertiesOriginal ValueComments
Blowing Agent Content 1.5 %
 3.0 - 5.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 53.0 MPa
@Thickness 6.35 mm
ASTM D638
Elongation at Break 7.8 %
@Thickness 6.35 mm
ASTM D638
Flexural Yield Strength 75.0 MPa
@Thickness 6.40 mm
ASTM D790
Flexural Modulus 1930 MPa
@Thickness 6.40 mm
ASTM D790
Izod Impact, Unnotched 2670 J/m
@Thickness 6.40 mm
ASTM D4812
Dart Drop, Total Energy 122 JSABIC method
Instrumented Impact Total Energy 8.00 J
@Temperature -40.0 °C
ASTM D3763
 67.0 J
@Temperature -20.0 °C
ASTM D3763
Tangent Modulus 2300 MPa
@Thickness 6.40 mm
ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+16 ohm-cmASTM D257
Surface Resistance >= 1.10e+17 ohmASTM D257
Dielectric Constant 2.47
@Frequency 100 Hz
ASTM D150
 2.68
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.0037
@Frequency 100 Hz
ASTM D150
 0.0039
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI >= 120 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.8 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E 831
Specific Heat Capacity 1.18 J/g-°CASTM C 351
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness 3.91 mm
UL 94
 V-1
@Thickness 5.99 mm
UL 94
Oxygen Index 28.2 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 260 °C
Middle Barrel Temperature 295 - 315 °C
Front Barrel Temperature 295 - 315 °C
Nozzle Temperature 280 - 305 °C
Melt Temperature 290 - 310 °C
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 105 °CBlowing Agent
 120 °CResin
Dry Time 3.00 - 4.00 hourResin
 4.00 hourBlowing Agent
 48.0 hourResin, Cumulative
 
Descriptive Properties
ELECTRICAL20 %
FLAME CHARACTERISTICS0.94 g/cm³
IMPACT10 %
MECHANICAL10 %
PHYSICAL10 %
Structural Foam MoldingFLC298
 Nitrogen Gas
THERMAL10 %

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® 3027IR Polycarbonate
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance
Covestro Makrolon® ET3227 Polycarbonate

PSABI21848 / 214984

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.