Compound 3725 is a 70 durometer white colored Buna N elastomer, it is formulated with FDA sanctioned materials. It exhibits good resistance to petroleum based oils a medium temperature. This compound is suitable for milk and edible oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 712 EO14 EO34; 2 BG 712 EO14 EO34 EA14 EF11 EF21; 5 BG 710 A14 EO14 EO34 3-A Sanitary Standards 18-03 Class lll & lV CFR 21 177.2600 This Compound is RoHS Compliant Information provided by Pressure Seals Inc. |