Ultradur B 4450 G5 is a 25% glass reinforced injection molding PBT for parts requiring enhanced fire resistance as well as increased tracking resistance. (Halogen and Antimon free) Applications: Typical applications include lamp sockets, connectors, coil formers, housings for control units, and power switches. Information provided by BASF. |