MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Eastman Synergex™ T
Categories: Fluid

Material Notes: Product Description: Synergex™ T is available as a colorless to light yellow liquid with a slight odor. This high-performance tertiary amine additive is capable of boosting the performance of metalworking fluids. Synergex™ T is a low-odor and low VOC N-alkylalkanolamine ideal for use as a neutralizing agent in semi-synthetic and full-synthetic emulsion lubricants wherein VOC and/or secondary amine issues are a concern. With very low vapor pressure and volatility, Synergex™ T allows for significantly extended fluid life. The Synergex product line, which includes Synergex™, Synergex™ T and Synergex™ T Plus, greatly enhance the performace of metal working fluid coolants, providing excellent corrosion protection, coupling performance and extended fluid line. Designed to meet the specific demands of the metalworking fluid market, the Synergex range comprises products that provide extended fluid life, offer enhanced lubricity, have low odor and are harmless. Eastman delivers several amine additives to the power transfer and functional fluid makets, enabling the formulation of products with stable pH throughout the working life of the fluid.

Application/Uses:

  • Metalworking and functional fluids
Key Attributes:
  • Completely water soluble
  • Enhanced emulsion stability
  • Excellent HES profiles
  • Low odor, low volatility and high flash point
  • Outstanding corrosion inhibition properties
  • Outstanding coupling agent

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 - 0.980 g/cc
Viscosity 100 cP
@Temperature 15.0 °C
Molecular Weight 161.3 g/mol
Vapor Pressure 0.00000980 atm
 
Thermal PropertiesOriginal ValueComments
Melting Point -70.0 °CFreezing Point
Boiling Point 283 °C@ 760 mm Hg
Flash Point 141 °CClosed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.462 - 1.468

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5594 / 222788

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.