MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® PZ0042E PA6-GF20 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Starflam PZ0042E is a glass filled, flame retardant PA6 for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccDAM; ISO 1183
Water Absorption 1.7 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.8 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50% RH; ISO 527-2
 87.0 MPaDAM; ISO 527-2
Elongation at Break 3.2 %DAM; ISO 527-2
 11 %50% RH; ISO 527-2
Tensile Modulus 2800 MPa50% RH; ISO 527-2
 5900 MPaDAM; ISO 527-2
Flexural Strength 52.0 MPa50% RH; ISO 178
 136 MPaDAM; ISO 178
Flexural Modulus 2500 MPa50% RH; ISO 178
 5800 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 3.70 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 3.90 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 4.50 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 4.70 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 9.10 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 32.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 33.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 35.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 48.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 78.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 3.60 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 3.80 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 3.90 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 3.90 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 4.20 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 9.80 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 27.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
High Voltage Arc Resistance to Ignition (HVAR) >= 120 sec
@Thickness 0.750 mm
UL 746
 >= 120 sec
@Thickness 0.800 mm
UL 746
 >= 120 sec
@Thickness 1.00 mm
UL 746
 >= 120 sec
@Thickness 1.50 mm
UL 746
 >= 120 sec
@Thickness 3.00 mm
UL 746
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness 0.750 mm
UL 746
 >= 120 arcs
@Thickness 0.800 mm
UL 746
 >= 120 arcs
@Thickness 1.00 mm
UL 746
 >= 120 arcs
@Thickness 1.50 mm
UL 746
 >= 120 arcs
@Thickness 3.00 mm
UL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CUnannealed; 50% RH; ISO 75-2/B
 215 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 169 °CUnannealed; 50% RH; ISO 75-2/A
 192 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 125 °C
@Thickness 0.750 mm
UL 746
 125 °C
@Thickness 0.800 mm
UL 746
 125 °C
@Thickness 1.00 mm
UL 746
 125 °C
@Thickness 1.50 mm
UL 746
 125 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 125 °C
@Thickness 0.750 mm
UL 746
 125 °C
@Thickness 0.800 mm
UL 746
 125 °C
@Thickness 1.00 mm
UL 746
 125 °C
@Thickness 1.50 mm
UL 746
 125 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 0.800 mm
UL 746
 130 °C
@Thickness 1.00 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 V-2
@Thickness 0.800 mm
UL 94
 V-2
@Thickness 1.50 mm
UL 94
 V-2
@Thickness 3.00 mm
UL 94
Glow Wire Ignition Temperature 725 °C
@Thickness 1.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 240 °CInjection
 <= 250 °CInjection
Middle Barrel Temperature >= 250 °CInjection
 <= 260 °CInjection
Front Barrel Temperature >= 250 °CInjection
 <= 270 °CInjection
Melt Temperature >= 250 °CInjection
 <= 270 °CInjection
Mold Temperature >= 50.0 °CInjection
 <= 90.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9124 / 287575

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.