MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATSP Innovations NOWE™ ATSP-11 Copolyester (unfilled)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: KEY CHARACTERISTICS:
  • Extremely low friction
  • Low surface energy
  • Great wear properties and high toughness
  • Good weathering resistance
  • Excellent oxidative stability
  • High glass transition and heat deflection temperature
  • Non-flammable
  • Cryogenic-safe
  • Very low moisture pickup and high moisture resistance
  • Easy machinability – low dust
APPLICATIONS:
  • Semiconductor machinery components
  • Valves and fittings
  • Bearings and bushings
  • Aerospace parts
  • Electrical components
  • Seals
  • Pump components

    This data was provided by ATSP Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/cc
Surface Tension 36 dynes/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 83
Tensile Strength 88.0 - 104 MPaASTM D883
Elongation at Break 2.5 - 3.5 %ASTM D883
Tensile Modulus 4.35 GPaASTM D883
Compressive Strength 292.7 - 314.9 MPaASTM D695
Izod Impact Resistance 0.336 J/cm²ASTM D256
Limiting Pressure Velocity >= 17.8 MPa-m/sec
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.0
@Frequency 1000 Hz
Dielectric Strength 385 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°C
Specific Heat Capacity 1.44 J/g-°C
@Temperature 25.0 °C
Thermal Conductivity 0.100 W/m-K
Maximum Service Temperature, Air 350 °C
Maximum Service Temperature, Inert 425 °C
Glass Transition Temp, Tg 261 °C
Oxygen Index 40 %
 
Descriptive Properties
ColorTranslucent; Red to brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Eastman Eastar MN211 Copolyester, Natural
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Armacell ArmaFORM® GR150 PET foam core

PESTHR01 / 243004

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.