MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 1527T Silicone Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 1527T is translucent in color RTV silicone. It has good weather resistance and excellent electrical insulation properties, especially resistant to sulfur hexafluoride and transformer oil. Typical application include electrical insulation, protecting leads from mechanical shock, bonding trim, sealing ductwork, vents, flues, doors, windows, and sealing and waterproofing of transformers.

Features and Benefits:

  • Excellent heat resistance properties
  • Wide operating temperature range
  • Easy to use for reworkable applications
  • Fast setting one component material
  • Neutral cure low/no odor
  • UL94 rated

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ISO 7619
Tensile Strength 1.30 MPaISO 37
 1.40 MPa
@Temperature 175 °C,
Time 605000 sec
Heat Aging; ISO 37
Elongation at Break 350 %ISO 37
 310 %
@Temperature 175 °C,
Time 605000 sec
Heat Aging; ISO 37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+14 ohm-cmIEC 60093
Dielectric Strength 18.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 15.0 minTack Free
 24.0 hour
@Thickness >=2.00 mm
Full Cure
 
Descriptive Properties
ColorTranslucent
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL149 / 316940

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.