MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Danquinsa DANADD® 100 Anti blocking and demoulding additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® 100 is a new, very effective anti blocking- and demoulding additive batch based on Nano-special wax. DANADD®100 will be added to the thermoplastic polyurethanes of the PEARLTHANE range if there are demoulding problems and a much to strong stickiness. The addition quantity is very little and will be normally around 0,3% to 1,5% . Often it will be sufficient to add this batch to the TPU’s only by the start of production and when changing the mould. In many cases only after the wetting of the tools a very good demoulding is reached.

Application: DANADD® 100 is added to the divers PEARLTHANE®- TPU’s (based on polyether, polyester and Polycaprolactone polyester) by injection moulding processing. With the addition of DANADD® 100 the stickiness on the surface will be reduced and a very good demoulding behaviour is reached. DANADD® 100 is chemically structured to avoid any disadvantage by the injection moulded parts or parts processed by extrusion, like it is the case with commonly used release agents. The processed parts can be very good lacquered, adhered etc. If the before mentioned addition of DANADD® 100 is made it won’t come to any migration by the processed parts. Further, there won’t be any disadvantages taken the colouration or any optical aspect if DANADD® 100 is added in the recommended quantity.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Active content76-84%MQSA-Nr.: 39a
Aspectlight grey, adhere granules
Dosage0,3 to 1,5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ000 / 294420

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.