MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Amodel® AE-1133 PPA, 33% glass filled
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass filled, for Auto EE, heat stabilized

Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin.

- Black: AE-1133 BK 324
- Natural: AE-1133 NT

Applications: Automotive Electronics; Connectors; Electrical Parts; Electrical/Electronic Applications

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Injection notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³Method A; ISO 1183
Water Absorption 0.21 %
@Time 86400 sec
0.21 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D785
Tensile Strength at Break  72.0 MPa
@Temperature 175 °C
10400 psi
@Temperature 347 °F
ISO 527-2
 80.0 MPa
@Temperature 150 °C
11600 psi
@Temperature 302 °F
ISO 527-2
 148 MPa
@Temperature 100 °C
21500 psi
@Temperature 212 °F
ISO 527-2
 233 MPa
@Temperature 23.0 °C
33800 psi
@Temperature 73.4 °F
ISO 527-2
Tensile Strength 221 MPa32100 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
 2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
ISO 527-2
 2.9 %
@Temperature 100 °C
2.9 %
@Temperature 212 °F
ISO 527-2
 8.5 %
@Temperature 175 °C
8.5 %
@Temperature 347 °F
ISO 527-2
 8.7 %
@Temperature 150 °C
8.7 %
@Temperature 302 °F
ISO 527-2
Tensile Modulus 13.1 GPa1900 ksiASTM D638
 4.30 GPa
@Temperature 175 °C
624 ksi
@Temperature 347 °F
ISO 527-2
 6.70 GPa
@Temperature 150 °C
972 ksi
@Temperature 302 °F
ISO 527-2
 10.8 GPa
@Temperature 100 °C
1570 ksi
@Temperature 212 °F
ISO 527-2
 13.4 GPa
@Temperature 23.0 °C
1940 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 317 MPa46000 psiASTM D790
 80.0 MPa
@Temperature 175 °C
11600 psi
@Temperature 347 °F
ISO 178
 93.0 MPa
@Temperature 150 °C
13500 psi
@Temperature 302 °F
ISO 178
 227 MPa
@Temperature 100 °C
32900 psi
@Temperature 212 °F
ISO 178
 319 MPa
@Temperature 23.0 °C
46300 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 11.4 GPa1650 ksiASTM D790
 3.60 GPa
@Temperature 175 °C
522 ksi
@Temperature 347 °F
ISO 178
 4.00 GPa
@Temperature 150 °C
580 ksi
@Temperature 302 °F
ISO 178
 9.80 GPa
@Temperature 100 °C
1420 ksi
@Temperature 212 °F
ISO 178
 11.6 GPa
@Temperature 23.0 °C
1680 ksi
@Temperature 73.4 °F
ISO 178
Compressive Strength 185 MPa26800 psiASTM D695
Poissons Ratio 0.410.41ASTM E132
Shear Strength 101 MPa14600 psiASTM D732
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
Izod Impact, Unnotched 7.70 J/cm14.4 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 8.80 kJ/m²4.19 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 49.0 kJ/m²23.3 ft-lb/in²Type 1; ISO 180
Charpy Impact Unnotched 7.30 J/cm²34.7 ft-lb/in²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 0.950 J/cm²4.52 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
ASTM D150
 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm
@Thickness 3.20 mm
533 kV/in
@Thickness 0.126 in
ASTM D149
Dissipation Factor  0.0050
@Frequency 60 Hz
0.0050
@Frequency 60 Hz
ASTM D150
 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 140 sec140 secASTM D495
Comparative Tracking Index 550 - 600 V550 - 600 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  24.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.3 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
 27.0 µm/m-°C
@Temperature 100 - 200 °C
15.0 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature 0.000 - 100 °C
30.6 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
 110 µm/m-°C
@Temperature 100 - 200 °C
61.1 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Melting Point 313 °C595 °FISO 11357-3
 313 °C595 °F
Maximum Service Temperature, Air 164 - 185 °C327 - 365 °FContinuous; ASTM D794
Deflection Temperature at 0.46 MPa (66 psi) 297 °C
@Thickness 3.20 mm
567 °F
@Thickness 0.126 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FUnannealed; ISO 75-2/A
 285 °C
@Thickness 3.20 mm
545 °F
@Thickness 0.126 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 - 318 °C579 - 604 °F
Front Barrel Temperature 316 - 329 °C601 - 624 °F
Melt Temperature 321 - 343 °C610 - 649 °FInjection
Mold Temperature 135 °C275 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content <= 0.045 %<= 0.045 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
Part Marking Code [ISO 11469]>PA6T/6I/66-GF33<
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4067 / 279867

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.