MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL8454 PC/Siloxane (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Siloxane

Material Notes: LEXAN EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color variability and contamination risks including black specs needs to be considered before approval for use in applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
SABIC method
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPaType I, 50. mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPaType I, 50 mm/min; ASTM D638
Elongation at Break 100 %Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2100 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 800 J/mASTM D256
 650 J/m
@Temperature -40.0 °C
ASTM D256
 700 J/m
@Temperature -30.0 °C
ASTM D256
Charpy Impact, Notched 65.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 67.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 27.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 54.0 kJ/m²
@Temperature -40.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 58.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 70.0 JASTM D3763
Tangent Modulus 2200 MPa5 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 0.800 mm
in oil; ASTM D149
Dissipation Factor 0.0093
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness 0.750 mm
UL 94
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 1 270 - 295 °C
Zone 2 280 - 305 °C
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °C
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °C
Dry Time 3.00 - 4.00 hour
 48.0 hourCumulative
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI21942 / 215078

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.