MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Trimet® 259 (Plymetal® A50N) Silver base Braze Filler Composite (AWS BAg-24)
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Trimet 259 is a three layer composite metal sandwich consisting of a copper core clad on each side with Silvaloy 505 alloy. The relative thicknesses of the three layers are in a 1/2/1 ratio. Other relative thickness ratios can be produced for special applications, if needed. Trimet 259 is useful for brazing large carbide tools inserts with braze surface areas in excess of 0.5in2 or linear dimension over 0.75 in. This product is used as pre-placed shim at the interface of the parts being joined.

Available forms: strip, engineered preforms, specialty preforms.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 1220 - 1305 °F
Solidus 1220 °F
Liquidus 1305 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1305 - 1550 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 19 - 21 %
 >= 99.9 %core
Nickel, Ni 1.5 - 2.5 %
Other, total <= 0.15 %
Silver, Ag 49 - 51 %
Zinc, Zn 26 - 30 %
 
Descriptive Properties
Braze Filler MetalSilvaloy 505Clad portion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9848 / 254793

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.