MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® G-7452 Fluoroelastomer Copolymer, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-7452 is a cure-incorporated copolymer with medium Mooney viscosity. It has excellent mold flow compared with fluoroelastomers of similar Mooney viscosity, making it well suited for compression, transfer or injection molding. DAI-EL® G-7452 is designed for seals and other complex shapes, where higher elongation at molding temperatures provides easy part demolding.

Typical Applications: Shaft seals, gaskets, molded tubing

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Rheological Properties ODR:
Temperature: 177°C
Frequency: 100 cpm
Strain: 3 °
Test time: 12 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/cc
Mooney Viscosity 42
@Temperature 121 °C
42
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373MDR 2000
 7474ODR
Tensile Strength at Break 15.0 MPa2180 psiODR
 15.3 MPa2220 psiMDR 2000
Elongation at Break 250 %250 %MDR 2000
 260 %260 %ODR
100% Modulus  4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
ODR
 4.70 MPa
@Strain 100 %
682 psi
@Strain 100 %
MDR 2000
Compression Set  15 %
@Temperature 200 °C,
Time 252000 sec
15 %
@Temperature 392 °F,
Time 70.0 hour
#214 O-ring, MDR 2000; ASTM D395 Method B
 17 %
@Temperature 200 °C,
Time 252000 sec
17 %
@Temperature 392 °F,
Time 70.0 hour
#214 O-ring, ODR; ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -18.0 °C-0.400 °FLow Temperature Retraction; ASTM D1329
 
Processing PropertiesMetricEnglishComments
Cure Time 1.50 min0.0250 hourts2, scorch time, MDR 2000
 1.90 min0.0317 hourt'50, time to 50% cure, MDR 2000
 2.10 min0.0350 hourts2, scorch time, ODR
 2.70 min0.0450 hourt'90, time to 90% cure, MDR 2000
 3.50 min0.0583 hourt'50, time to 50% cure, ODR
 4.00 min0.0667 hourt'90, time to 90% cure, ODR
 5.00 min
@Temperature 177 °C
0.0833 hour
@Temperature 351 °F
Press Cure, ODR
 10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
Press Cure, MDR 2000
 1440 min
@Temperature 232 °C
24.0 hour
@Temperature 450 °F
Post Cure, MDR 2000
 1440 min
@Temperature 260 °C
24.0 hour
@Temperature 500 °F
Post Cure, ODR
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %
 
Descriptive Properties
ColorWhite to cream
MH19.1 dNmmaximum torque, MDR 2000
 97 dNmmaximum torque, ODR
ML1.2 dNmminimum torque, MDR 2000
 12 dNmminimum torque, ODR
Test Formula100 phrDAI-EL® G-7452
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9839 / 209910

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.