MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC PPcompound 8900 PP (Europe)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: SABIC® PPcompound 8900 is a mineral filled modified polypropylene. This material combines high flow with a very high stiffness and high impact, as well as a very low shrinkage and CLTE. The high stiffness and low CLTE makes the material suited for high demanding applications. Typical applications include automotive exterior parts such as large thin wall zero gap bumper designs and (offline painted) vertical body panels. It can be used in painted and unpainted applications with UV stabilization added on demand. SABIC® PPcompound 8900 is a designated automotive grade. IMDS ID: 62202096

Information provided by Sabic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Filler Content 25 %SABIC method
Linear Mold Shrinkage 0.0060 cm/cm
@Time 86400 sec
SABIC method
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.0 MPaISO 527/1A
Tensile Strength, Yield 24.0 MPaISO 527/1A
Elongation at Break 50 %ISO 527/1A
Tensile Modulus 2600 MPaISO 527/1A
Flexural Modulus 2300 MPaISO 178/1A
Izod Impact, Notched (ISO) 30.0 kJ/m²ISO 180/1A
 3.50 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 7.00 kJ/m²
@Temperature 0.000 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 50.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
 55.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI31506 / 229426

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.