MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Persian Gulf Polymer LLDPE-LL22B01AA
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: 22B01 is a LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels and it is well suited for blending with LDPE and for general purpose applications. Application: High stiffness Blown film, Blending, Lamination. Features: High stiffness Blown film, Blending, Lamination. Additives: Thermal Antioxidant (Process Stabilizer), Anti-block agent, Processing aid.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 - 0.924 g/cc0.0332 - 0.0334 lb/in³ASTM D1505
Melt Flow 0.80 - 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 800 %800 %ASTM D882
Film Elongation at Break, TD 900 %900 %ASTM D882
2% Secant Modulus 0.150 GPa21.8 ksiMD; ASTM D882
 0.180 GPa26.1 ksiTD; ASTM D882
Elmendorf Tear Strength MD 120 g120 gASTM D1922
Elmendorf Tear Strength TD 400 g400 gASTM D1922
Dart Drop Test 75.0 g0.165 lbASTM D1709
Film Tensile Strength at Break, MD 49.0 MPa7110 psiASTM D882
Film Tensile Strength at Break, TD 43.0 MPa6240 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 25 %25 %ASTM D1003
Gloss 35 %35 %45°; ASTM D2457
Yellow Index 0.50 %0.50 %ASTM D1925
 
Descriptive Properties
F/E Ratio<30ASTM D1238
Fish Eye Note60 Gels/m2MTM 17108
Titanium Content (%)2Pgm wt; MTM 15636

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI971 / 250375

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.