Product Description: Hydrolysis Resistant, Heat Stabilized, 40% Glass Reinforced, Polyamide 6 Resin ID (ISO 1043): PA6–GF05 Filler / Reinforcement: Glass Fiber, 5% Filler by Weight Processing: Injection Molding Color: Natural Information provided by Petropol |