MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Tribocomp® PA66 LGF35 S9 MoS2 Polyamide 66 (Nylon 66), 35% Long Glass Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Tribocomp® PA66 LGF35 S9 MoS2 is a 35% long glass fiber reinforced high-flow PA66 with a pellet length of 9mm and MoS2. It can easily be processed on most injection molding machines.

Key Attributes: Abrasion Resistant; Heat Stabilized; High Flow; High Temperature Strength; Low Shrinkage; Medium Friction

Applications: Automotive Applications; Automotive Under the Hood; Engineering Parts; Gears; Industrial Applications; Power/Other Tools

Injection Notes: Pre-drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried.

Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 15%, and only regrind of optimum quality should be used. In any case, part properties should be checked.

Data for dry samples unless noted.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
Moisture Absorption 1.40 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 125 MPa
@Temperature 120 °C
ISO 527-2
 145 MPa
@Temperature 90.0 °C
ISO 527-2
 175 MPa
@Temperature 23.0 °C
Conditioned; ISO 527-2
 215 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 3.0 %ISO 527-2
Tensile Modulus 7200 MPa
@Temperature 120 °C
ISO 527-2
 8200 MPa
@Temperature 90.0 °C
ISO 527-2
 9300 MPa
@Temperature 23.0 °C
Conditioned; ISO 527-2
 12200 MPa
@Temperature 23.0 °C
ISO 527-2
Flexural Strength 340 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 11500 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°CISO 11359-2
Thermal Conductivity 0.310 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 255 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 253 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 - 300 °C
Middle Barrel Temperature 270 - 300 °C
Front Barrel Temperature 285 - 300 °C
Nozzle Temperature 285 - 310 °C
Melt Temperature <= 300 °C
Mold Temperature 80.0 - 160 °C
Drying Temperature 100 °C
@Time 14400 sec
Moisture Content <= 0.10 %
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
ColorBlack
FormsPellets
Suggested Max Regrind Injection (%)15

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y5442 / 238823

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.