MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials GE Sealants & Adhesives Paintable Silicone All Projects Window & Door 100% waterproof sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Paintable Silicone All Projects Window & Door sealant is a high-performance sealant with a hybrid formulation that combines the outstanding waterproof performance you would expect from a silicone sealant with the ease of use and paintability of an acrylic latex. This 100% waterproof sealant is ideal for a range of exterior and weatherproofing projects and can be exposed to water or painted in as little as 30 minutes. Paintable Silicone All Projects sealant offers 7-year mold-free product protection, goes on smoothly, and is easy to tool. This flexible and durable sealant will not crack or crumble over time. Backed by a lifetime guarantee.

Features: Hybrid performance, waterproof and paintable. 100% waterproof. 30-minute rain-ready. 30-minute paint-ready. Resists mold with 7-year mold-free product protection. Permanent flexibility. Excellent adhesion to wet or dry surfaces. Shrink & crack-proof. Low odor. Meets ASTM C-920 Class 25 specifications. Lifetime guarantee.

Applications: Paintable Silicone All Projects Window & Door sealant is used in a wide variety of applications including windows, doors, siding, trim, decks, lattice, soffits, and vents.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccCured.
 1.40 g/cc1.40 g/ccCured.
Volatile Organic Compounds (VOC) Content 11 g/l11 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 <= 21 g/l<= 21 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2929ASTM D2240
Tensile Strength 0.896 MPa130 psiASTM D412
Elongation at Break 210 %210 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.6 °C150 °F
 121 °C250 °F
Minimum Service Temperature, Air -59.4 °C-75.0 °F
 -34.4 °C-30.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour1/4" deep section.
 7200 - 10100 min120 - 168 hourFull Cured. Most common bead sizes.
Tack-Free Time  30.0 min
@Temperature 22.2 °C
0.500 hour
@Temperature 72.0 °F
ASTM C679
 60.0 min
@Temperature 22.2 °C
1.00 hour
@Temperature 72.0 °F
ASTM C679
Working Life 20.0 min20.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColorCrystal clearM90033
 WhiteGE7000
Consistency / Sag< 0.01 inchesASTM D2202
Joint Movement Capability±25%ASTM C719.
OdorLow
Rain Ready30 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9954 / 265769

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.