MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC Lexan® FXD9945A PC  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall applications.

This data was supplied by SABIC-IP for the Americas region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D 792
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 0.15 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66.0 MPaType I, 50 mm/min; ASTM D 638
 68.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPaType I, 50 mm/min; ASTM D 638
 66.0 MPa50 mm/min; ISO 527
Elongation at Break 120 %Type I, 50 mm/min; ASTM D 638
 120 %50 mm/min; ISO 527
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D 638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2370 MPa1 mm/min; ISO 527
 2380 MPa5 mm/min; ASTM D 638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 102 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2250 MPa2 mm/min; ISO 178
 2450 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 110 J/m
@Temperature -30.0 °C
ASTM D 256
 820 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
 70.0 kJ/m²
@Temperature 23.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
 73.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 79.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 73.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 140 °CRate B/50; ISO 306
 141 °CRate B/120; ISO 306
 143 °CRate B/50; ASTM D 1525
Flammability, UL94 V-0
@Thickness 2.00 mm
UL 94
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPASSESIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABIC2535 / 116423

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.