MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PRE-ELEC® PA 1406  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 has an excellent balance of mechanical properties and is easy to injection mould.

Typical applications include injection molded technical parts and housings for electronic components and other static sensitive devices (SSD) when high rigidity is needed.

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Linear Mold Shrinkage 0.0040 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868
Tensile Strength, Yield 92.0 MPaISO 527
Elongation at Break 10 %ISO 527
Modulus of Elasticity 5.00 GPaISO 178
Izod Impact, Notched 50.0 J/m
@Thickness 4.00 mm,
Temperature -20.0 °C
ISO 180
 500 J/m
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
Izod Impact, Unnotched 1.25 J/cm
@Thickness 4.00 mm,
Temperature -20.0 °C
ISO 180
 5.30 J/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1e+05ISO D-257
Surface Resistance <= 1.00e+7 ohmISO D-257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 208 °CISO 75/Method Bf
Vicat Softening Point 217 °CRate A; ISO 306/A50
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
Pre-drying in a dehumidifier
Moisture Content <= 0.15 %When Produced
Injection Pressure 8700 - 11600 psi
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
ColorBlack
Injection SpeedModerate

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
RTP Company RTP 199 X 70815  Polypropylene (PP) Long Glass Fiber 30% - Chemically Coupled - Heat Stable
Overview of materials for PVC, Rigid Grade
LNP Stat-Kon® RC-1003 Polyamide 66, Carbon Fiber Reinforcement
Ensinger TECASINT 1011 Polyimide (PI)

PPREMA028 / 58041

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.