Description: APPEX14 is a pre-grafted polyethylene which can be processed in combination with its catalyst master batch (APCAT12N) in conventional extruders. Cross linking happen by exposing end products to moisture. It's used for domestic hot and cold water, under floor heating and central heating.Information provided by Abhar Polymer Compounds |