MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT ACC18 Silicone coating
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: ACC18 is a fast curing, low viscosity, 1-component, condensation curing silicone coating. The uncured product can be applied by pouring, brushing or spraying and is readily cured to a tough, transparent rubber. It can be used to coat printed circuit boards to prevent ingress of water and environmental contaminants.

Key Features

  • Fast Room temperature cure
  • Low viscosity
  • Fluorescent UV aid for Production QA checks
  • Excellent adhesion to many substrates
  • Excellent adhesion to Humiseal 1.94V-0 boards
  • Low odor
  • RoHS compliant
Cured Elastomer: After 7 days at 23°C / 55 +/- 5% Humidity on a 3 mm thick test sheet

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D70
Brookfield Viscosity 260 cP
Storage Temperature 5.00 - 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 36ASTM D 2240-95
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+14 ohm-cmASTM D-257
Dielectric Constant 2.49
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength >= 457 V/milASTM D-149
Dissipation Factor 0.00060ASTM D-150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 310 µm/m-°C
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 6.00 minTack free time; AMB 001
 16.0 minCure to 300 µm
Shelf Life 12.0 Month
 
Descriptive Properties
ColorPale yellow
RheologyLiquid
Volume Coefficient of Thermal Expansion930 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL167 / 314650

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.