Synthetic single crystal lead tin disulfide (PbSnS2) is a special member of layered transition metal dichalcogenides. The coupling between adjacent layers is weak and can be easily peeled off and separated into monolayers. In bulk, it has a bandgap of 1.45 eV. The physical properties of monolayer PbSnS2 are both theoretically and experimentally unknown. Synonyms: Lead Tin Disulfide Alfa Chemistry Materials product group: 2D Alloys Manufacturer data sheet |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |