VESTAMID LX9001 black 9.7504 is a heat stabilized and light resistant PA 12 compound especially developed for extrusion coating of steel tubes. Due to the exceptional impact strength, abrasion resistance, and good chemical resistance of PA 12, and the excellent adhesion between the steel and the properly applied VESTAMID LX9001 black 9.7504, the corrosion resistance of steel tubes coated with VESTAMID LX9001 black 9.7504 is significantly increased. Further advantages of VESTAMID LX9001 black 9.7504 are the characteristics of PA 12 little low water absorption, good dimensional stability and nearly unaffected properties in changing ambient humidity. VESTAMID LX9001 black 9.7504 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing. Property data for dry samples. Information provided by Evonik. |