MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Cool Cover™ TPO Edge Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: H.B. Fuller’s patented Cool Cover™ TPO Edge Sealant* is a high solids, low VOC, elastomer based white edge sealant designed to seal the exposed edges of TPO membrane splices and laps. The sealant has excellent adhesion to TPO membranes as well as various other substrates including EPDM, metal, wood, and concrete. The sealant can be used on TPO as well as EPDM roofing systems. Cool Cover™ TPO Edge Sealant is suitable for use in VOC regulated markets such as California and the O.T.C. States.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 84 %ASTM C 681
Volatile Organic Compounds (VOC) Content <= 250 g/lASTM D 2369
Storage Temperature 4.00 - 38.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
Minimum Service Temperature, Air -40.0 °C
Flash Point 10.0 °CASTM D 56
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hourTack free time; ASTM D 2377
 72.0 hourASTM D 2377
Shelf Life 24.0 Month
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL234 / 317025

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.