MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Samarium Oxide
Material Notes: Samarium Oxide, also called Samaria, Samarium has a high neutron absorption capacity, Samarium Oxides have specialized uses in glass, phosphors, lasers, and thermoelectric devices. Calcium Chloride crystals treated with Samarium have been employed in lasers which produce beams of light intense enough to burn metal or bounce off the moon. Samarium Oxide is used in optical and infrared absorbing glass to absorb infrared radiation. Also, it is used as a neutron absorber in control rods for nuclear power reactors. The Oxide catalyzes dehydration of acyclic primary alcohols to aldehydes and ketones. Another use involves preparation of other Samarium salts.

Applications: also called Samaria, Samarium has a high neutron absorption capacity, Samarium Oxides have specialized uses in glass, phosphors, lasers, and thermoelectric devices. Calcium chloride crystals treated with samarium have been employed in lasers which produce beams of light intense enough to burn metal or bounce off the moon.

Solubility: Insoluble in water, moderately soluble in strong mineral acids

Molecular Formula: Sm2O3

Alfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.347 g/cc0.3016 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
Molecular Weight 349 g/mol349 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 2325 °C4217 °F
 
Descriptive Properties
AppearanceLight Yellowish
CAS Number12060-58-1
Purity99.999% 99.99% 99.9% 99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA66672 / 304791

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.