MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ DX10311 PC (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D 792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 37 g/10 min
@Load 5.00 kg,
Temperature 300 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 117 MPaType I, 5 mm/min; ASTM D 638
 119 MPa5 mm/min; ISO 527
Elongation at Break 2.6 %Type I, 5 mm/min; ASTM D 638
 2.7 %5 mm/min; ISO 527
Tensile Modulus 8260 MPa1 mm/min; ISO 527
 8330 MPa5 mm/min; ASTM D 638
Flexural Strength 181 MPa2 mm/min; ISO 178
 190 MPaASTM D 790
Flexural Yield Strength 182 MPa2 mm/min; ISO 178
Flexural Modulus 7670 MPaASTM D 790
 7720 MPa2 mm/min; ISO 178
Izod Impact, Notched 196 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 752 J/m
@Temperature 23.0 °C
ASTM D 4812
Charpy Impact Unnotched 57.0 kJ/m²
@Temperature 23.0 °C
ISO 179/2C
Charpy Impact, Notched 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179/2C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
@Thickness 3.20 mm
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI48254 / 189339

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.