MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Commercial Bronze, UNS C22000 (90-10 Bronze), OS035 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.035 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Coining; Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical uses: Etching Bronze; Grill Work; Ornamental Trim; Screen Cloth; Weather Stripping; Hardware; Kick Plates; Ball Point Pens; Caskets; Chain Links; Compacts; Costume Jewelry; Housing for Lipstick Compacts; Lipstick Cases; Cable Wrap; Rotor Bar - AC Motors; Wave Guides; Bolts; Line Clamps; Rivets; Screw Shells; Screws; Base for Vitreous Enamel; Escutcheons; Flexible Tube; Screen Wire; Studs; Marine Hardware; Artillery Projectile Rotating Bands, Press Fit; Primer Caps; Rotating Bands; Small Arms Cartridges

Applicable Specifications: Bands - Projectile Rotating MILITARY MIL-B-18907, Projectile Rotating MILITARY MIL-B-20292; Bar – SAE J463, SAE J461, ASTM B36/B36M; Cups – ASTM B131, MILITARY MIL-C-3383; Plate – ASTM B36/B36M; Rod, Bar & Shapes – ASTM B927/B927M; Seamless Tube – ASME SB135, ASTM B135/B135M, ASTM B135; Sheet – ASTM B694, SAE J463, SAE J461, ASTM B36/B36M; Strip – ASTM B36/B36M, SAE J461, ASTM B130, SAE J463, ASTM B694; Tube – SAE J461, ASTM B587, Rectangular Waveguide ASTM B372, Rectangular Waveguide MILITARY MIL-W-85, SAE J463; Wire – ASTM B134/B134M, MILITARY MIL-W-6712

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.318 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 57
Hardness, Rockwell 30T 12
Tensile Strength 38.0 ksi
Tensile Strength, Yield 12.0 ksi0.5% Ext
Elongation at Break 50 %
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000390 ohm-cm44% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.9 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 109 BTU-in/hr-ft²-°F
Melting Point 1870 - 1910 °F
Solidus 1870 °F
Liquidus 1910 °F
Annealing Point 800 - 1450 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 89 - 91 %
Lead, Pb <= 0.050 %
Zinc, Zn 8.9 - 11 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC22000x1 / 292890

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.