MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Kazanorgsintez Triethanolamine
Categories: Fluid; Solvent

Material Notes: Production Method: Grades A and B are obtained by ammonia oxyethylation, Grade 'Clarified' is achieved by purified monoethanolamine oxyethylation.

Application: Industrial triethanolamine is the component of rubber softeners, coolants, perfumes and cosmetics. Triethanolamine and highest fatty acids salts are used as detergents, emulsifying and wetting agents and lubricants. Triethanolamine is used also as an absorbent of acid gases, corrosion inhibitor, accessory material in cement production, and as a feed stock for a number of organic synthesis in the pharmaceutical industry.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.095 - 1.124 g/cc
@Temperature 20.0 °C
A Grade
 1.095 - 1.135 g/cc
@Temperature 20.0 °C
"Clarified" Grade, B Grade
 
Component Elements PropertiesOriginal ValueComments
Free Water <= 0.50 %A Grade
 <= 1.0 %B Grade
 <= 1.0 %"Clarified" Grade
 
Descriptive Properties
Appearance"Clarified" Grade: Viscous transparent liquid, opalescence is permissible from yellow to dark-brown color, greenish tone is allowable.

A Grade, B Grade: Transparent liquid, opalescence is achieved. Color from yellow to dark-brown, greenish case is allowed

Color50Hazen units, "Clarified" Grade
Mass Content (%)1Mass content of monoethanolamine, A Grade
 13Mass content of diethanolamine, B Grade
 2Mass content of monoethanolamine, B Grade
 85Mass content of triethanolamine, B Grade
 9Mass content of diethanolamine, A Grade
 90Mass content of triethanolamine, "Clarified" Grade, A Grade
 UnlimitedMass content of diethanolamine, "Clarified" Grade
 UnlimitedMass content of monoethanolamine, "Clarified" Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAZAN124 / 127443

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.